Review of Fe-6.5 wt% Si high silicon steel—A promising soft magnetic material for sub-kHz application

G Ouyang, X Chen, Y Liang, C Macziewski… - Journal of Magnetism and …, 2019 - Elsevier
To meet the growing need for energy efficiency in power electronics and electric machines,
a number of new soft magnetic materials are being investigated. Among them, high silicon …

[图书][B] Handbook of magnetic measurements

S Tumanski - 2016 - books.google.com
Collecting state-of-the-art knowledge from information scattered throughout the literature,
this handbook describes magnetic materials and sensors, the testing of magnetic materials …

Relationship between laser energy input, microstructures and magnetic properties of selective laser melted Fe-6.9% wt Si soft magnets

M Garibaldi, I Ashcroft, N Hillier, SAC Harmon… - Materials …, 2018 - Elsevier
Abstract Selective Laser Melting (SLM), a powder-bed Additive Manufacturing technology,
can be used in combination with high temperature post-annealing to produce high-silicon …

[PDF][PDF] Laser additive manufacturing of soft magnetic cores for rotating electrical machinery: materials development and part design

M Garibaldi, C Gerada, R Hague - 2018 - researchgate.net
Since its invention in the first half of the 19th Century, electrical machinery has established
itself as a fundamental component in several industrial sectors. In the form of motors …

Deformation twinning feature and its effects on significant enhancement of tensile ductility in columnar-grained Fe–6.5 wt.% Si alloy at intermediate temperatures

J Xie, H Fu, Z Zhang, Y Jiang - Intermetallics, 2012 - Elsevier
The tensile deformation behavior of columnar-grained Fe–6.5 wt.% Si alloy with< 100> fiber
texture at intermediate temperatures (300–500° C) was investigated. Compared with …

Effect of Al content on magnetic properties of Fe-Al Non-oriented electrical steel

J Hong, H Choi, S Lee, JK Kim, Y mo Koo - Journal of Magnetism and …, 2017 - Elsevier
The effects of Al content (0.53≤ Al≤ 9.65 wt%) on microstructure, texture, magnetic flux
density, permeability, core loss and magnetic domain structure of Fe-Al based electrical …

Improvement on room-temperature ductility of 6.5 wt.% Si steel by stress-relief annealing treatments after warm rolling

X Wang, W Zhang, Z Liu, H Li, G Wang - Materials Characterization, 2016 - Elsevier
In our previous work, we demonstrated that thin sheets of 6.5 wt.% Si steel could be
fabricated by cold rolling with deformation induced disordering (DID). However, because the …

Cold rolled Fe-6.5 wt.% Si alloy foils with high magnetic induction

XS Fang, YF Liang, F Ye, JP Lin - Journal of Applied Physics, 2012 - pubs.aip.org
Fe-6.5 wt.% Si alloy foils with 95 mm in width and 0.30 mm in thickness were successfully
fabricated by cold rolling process. Excellent magnetic properties (H c= 20.4 A/m, µ m= 22 …

Fabrication of Fe‐6.5 wt% Si Ribbons by Melt Spinning Method on Large Scale

YF Liang, S Wang, H Li, YM Jiang… - Advances in Materials …, 2015 - Wiley Online Library
Melt spinning method has been widely applied for fabrication of Fe‐based amorphous/
nanocrystalline ribbons in industry. Compared with Fe‐based amorphous/nanocrystalline …

Effect of Cu addition on microstructure, texture and magnetic properties of 6.5 wt% Si electrical steel

Z Cheng, J Liu, Z Xiang, J Jia, O Volkova… - Journal of Magnetism …, 2021 - Elsevier
The effect of Cu addition in the range of 0–1.0 wt% on the magnetic induction and iron loss
of 6.5 wt% Si electrical steel is investigated. The microstructure and texture of the steels are …