[HTML][HTML] Mechanical and wear behaviors of 316L stainless steel after ball burnishing treatment

S Attabi, A Himour, L Laouar… - Journal of Materials …, 2021 - Elsevier
The performance and durability of orthopedic implants are mainly determined by their
surface integrity. Ball burnishing (BB) is a kind of finishing treatment which improves the …

Effect of electroless Ni-B and Ni-WB coatings on the corrosion-fatigue behaviour of 7075 Al alloy

RA Yildiz, K Genel, T Gulmez - International Journal of Fatigue, 2021 - Elsevier
This research experimentally determines the effect of electroless Ni-B and Ni-WB coatings
on the fatigue and corrosion-fatigue life of 7075 Al alloy substrate. SEM, XRD, fracture …

Impact wear behavior of ball burnished 316L stainless steel

H Yilmaz, R Sadeler - Surface and Coatings Technology, 2019 - Elsevier
This study investigated the damage mechanism occurring in metallic materials working
under repeated impact loads. AISI 316L stainless steel was used as the test material. In …

A study on properties of electroless Ni-B/MgB2 coatings on AZ91 magnesium alloy

F Bülbül, T Kılcı - Heliyon, 2024 - cell.com
This study explores MgB 2 as a reinforcing agent in electroless deposition on AZ91
magnesium alloy substrates, evaluating its impact on coating properties. X-ray diffraction …

Effect of ball burnishing treatment on the fatigue behavior of 316L stainless steel operating under anodic and cathodic polarization potentials

H Yilmaz, R Sadeler - Metallurgical and Materials Transactions A, 2018 - Springer
Corrosion fatigue (CF) behavior of AISI 316L was investigated in a 3 pct NaCl aqueous
solution at an R=− 1 stress ratio and a frequency of 60 Hz at room temperature. The test …

[HTML][HTML] Surface Integrity of Ball Burnished 316L Stainless Steel

S Attabi, A Himour, L Laouar, A Motallebzadeh - Stainless Steels, 2022 - intechopen.com
Abstract 316L is a type of austenitic stainless steel that offers a good combination of
mechanical properties, corrosion resistance, and biocompatibility. In some industrial …

[引用][C] AISI 316L çeliğinin anodik ve katodik polarizasyon potansiyelleri altında korozyonlu yorulma ve darbeli aşınma davranışına bilye ile ezerek parlatma işleminin …

H Yilmaz - 2019 - Doktora Tezi, Atatürk Üniversitesi …