Failure analysis of convection section tube in an ethylene cracking furnace due to metal dusting

S Xiao, J Wang, C Huang, L Tian, W Su - Engineering Failure Analysis, 2023 - Elsevier
To study the failure in the convection section tubes of an ethylene cracking furnace,
macroscopic inspections, chemical composition analysis, metallographic microscopy …

[HTML][HTML] Tribocorrosion and metal release from austenitic stainless steels 304 and 201 in simulated cassava food contact

R Addai, TE Olowoyo, JD Henderson, TE Standish… - Tribology …, 2024 - Elsevier
Cassava is the third most significant calorie source in the tropics. Its processing has
changed from traditional methods to stainless steel processing machines. This study …

Evaluation of metal dusting resistance of thermal sprayed NiCrAlSiTaY and NiCrAlSiTaY/laser re-melted Al2O3 coatings on Inconel 625

AM Ardali, B Lotfi - Surface and Coatings Technology, 2022 - Elsevier
The present study assessed the resistance against MD corrosion in a single-layer, oxide-
forming NiCrAlSiTaY coating, and a double-layer NiCrAlSiTaY/laser-remelted (LRed) Al 2 O …

Simultaneous oxidation and carburization of a Fe-9Cr alloy under different oxygen pressures at 800 C

J Shen, S Liu, XH Guo, Y Niu - Corrosion Science, 2017 - Elsevier
A model Fe-9Cr alloy was exposed to various H 2 single bondCO 2 single bondCH 4
mixtures providing different oxygen pressures and carbon activities at 800° C. Three …

Atomic layer deposition of aluminum oxide on modified steel substrates

K Kukli, E Salmi, T Jõgiaas, R Zabels… - Surface and Coatings …, 2016 - Elsevier
Al 2 O 3 thin films were grown by atomic layer deposition to thicknesses ranging from 10 to
90 nm on flexible steel substrates at 300° C using Al (CH 3) 3 and H 2 O as precursors. The …

The features of metal dusting process in the extremely low nickel austenitic stainless steel (18Cr-21Mn-0.65 N-Fe)

S Kumar, GS Mahobia - Corrosion Science, 2020 - Elsevier
The features of metal dusting in extremely low nickel austenitic stainless steel (18Cr-21Mn-
0.65 N-Fe) were studied in syngas environment (75% H 2 and 25% CO) at 400-700° C …

Design of boiler welding for improvement of lifetime and cost control

A Thong-On, C Boonruang - Materials, 2016 - mdpi.com
Fe-2.25 Cr-1Mo a widely used material for headers and steam tubes of boilers. Welding of
steam tube to header is required for production of boiler. Heat affected zone of the weld can …

Development of Al oxide PVD coatings against metal dusting

E Uribe, O Salas, D Melo-Maximo… - Surface …, 2015 - journals.sagepub.com
Al oxide thin films were deposited on 304L stainless steel substrates to investigate their
potential as protective coatings in metal dusting environments. Deposition of the films was …

超高强度不锈钢10Cr13Co13Mo5Ni 3W1VE 微观组织对局部腐蚀行为的影响.

滕鹏, 钟锦岩, 匡效禹, 赵振江… - Journal of Materials …, 2024 - search.ebscohost.com
采用未时效, 200,400℃ 以及500℃ 时效状态下10Cr13Co13Mo5Ni3W1VE (S280)
马氏体超高强度不锈钢为研究对象, 通过X 射线衍射(XRD), 透射电子显微镜(TEM) …

Establishing the cause of failure in a secondary reformer nozzle in an ammonia plant

M Taghipour, A Bahrami, R Rahimzadeh… - Journal of Failure …, 2021 - Springer
In this study, the cause of a severe failure and degradation of a nozzle in a secondary