Achieving superb strength in single-phase FCC alloys via maximizing volume misfit

Z Li, S Ma, S Zhao, W Zhang, F Peng, Q Li, T Yang… - Materials Today, 2023 - Elsevier
Single-phase face-centered cubic (SP-FCC) alloys normally possess low strength.
Conventionally strengthening strategies inevitably cause significant ductility sacrifice. Here …

Recent progress of vanadium-based alloys for fusion application

SN Jiang, FJ Zhou, GW Zhang, XO Yi, CW Yu, XJ Wang… - Tungsten, 2021 - Springer
Low-activation vanadium alloys, with the reference composition of V–4Cr–4Ti have been
considered as one of the most promising candidate materials for structural components such …

[HTML][HTML] In situ neutron diffraction analysis of microstructural evolution-dependent stress response in austenitic stainless steel under cyclic plastic deformation

M Kumagai, M Kuroda, T Matsuno, S Harjo, K Akita - Materials & Design, 2022 - Elsevier
Understanding fatigue phenomena in metals is of great significance for mechanical
performance in engineering systems. Microstructural evolution in austenitic stainless steels …

In situ diffraction characterization on microstructure evolution in austenitic stainless steel during cyclic plastic deformation and its relation to the mechanical response

M Kumagai, K Akita, M Kuroda, S Harjo - Materials Science and …, 2021 - Elsevier
Diffraction line profile analysis was performed to qualitatively evaluate the change in the
microstructure of austenitic stainless steel during 250 cycles of plastic deformation. The …

Interfacial characterization of dissimilar-metals bonding between vanadium alloy and Hastelloy X alloy by explosive welding

S Jiang, J Shen, T Nagasaka, T Muroga… - Journal of Nuclear …, 2020 - Elsevier
Dissimilar-metals bonding between V–4Cr–4Ti and Hastelloy X alloy was investigated by
explosive welding, which is essential to connect coolant pipes of Flibe blanket and external …

The microstructure and mechanical properties of drawn and aged pearlitic steel wires

S Yamasaki - Materials Science and Technology, 2018 - Taylor & Francis
Cold-drawn pearlitic steel wires exhibit the highest strength amongst steel products for
commercially use. The microstructure and the mechanical properties of wires are influenced …

Bubbles and precipitates formation and effects on the hardening of irradiated vanadium alloys

S Jiang, C Yu, P Zheng, L Guo, X Zhou… - Journal of Nuclear …, 2021 - Elsevier
This paper investigated the formation of bubbles and precipitates and the hardening effects
in V–4Cr–4Ti alloy after irradiation of He and H ions and post-irradiation annealing …

One-step annealing optimizes strength-ductility tradeoff in pearlitic steel wires

L Xiang, LW Liang, YJ Wang, Y Chen, HY Wang… - Materials Science and …, 2019 - Elsevier
In this paper, the mechanical properties of a cold-drawn wire (ε= 2.43) are modulated by
simple annealing and the variation of its microstructure is characterized by transmission …

Characterization of dislocation rearrangement in FCC metals during work hardening using X-ray diffraction line-profile analysis

K Nakagawa, M Hayashi, K Takano-Satoh… - Quantum Beam …, 2020 - mdpi.com
Multiplication and rearrangement of dislocations in face-centered cubic (FCC) metals during
tensile deformation are affected by grain size, stacking fault energy (SFE), and solute …

Stress corrosion cracking mechanisms in bridge cable steels: Anodic dissolution or hydrogen embrittlement

Z Zhang, L Wang, W Huang, X Min, G Luo… - International Journal of …, 2025 - Elsevier
Two key mechanisms, anodic dissolution, and hydrogen embrittlement, govern the stress
corrosion cracking (SCC) in bridge cable steel wires. This study investigates the …