MA Atwater - Metal Powder Report, 2019 - magonlinelibrary.com
Although functional materials are not a new application for powder metallurgy (PM), renewed emphasis and constant development are creating new possibilities. For instance …
M Shehata Aly - Journal of materials engineering and performance, 2010 - Springer
Open-cell nickel foams with average pore size of 600 μm have been subjected to room temperature tensile tests to explore their tensile properties. Using a state of the art …
V Paserin, J Shu, AM Liu, BQ Yu… - … 2007: Porous Metals …, 2008 - books.google.com
Nickel foam has been widely used as electrodes in NiMH and NiCd batteries. In addition to the wide range of commercially available foam products, new grades of Ni-based foams with …
抄録 Several methods have been developed for producing high-porosity open-cell metal foams, but no method is available for producing closed-cell type metal foams with a porosity …
抄録 Production process of high porosity closed cell type metal foam is developed using a hydrogel binder. Using this process, the stainless steel foam is produced with its porosity …