Tungsten heavy alloys processing via microwave sintering, spark plasma sintering, and additive manufacturing: A review

R Manikandan, A Raja Annamalai - Processes, 2022 - mdpi.com
Highlights The dihedral angle and liquid content of WHA alloy greatly influence the alloy's
density. High densification and deformation were observed in the sample with high liquid …

Recent progress in processing of tungsten heavy alloys

Y Şahin - Journal of Powder Technology, 2014 - Wiley Online Library
Tungsten heavy alloys (WHAs) belong to a group of two‐phase composites, based on W‐Ni‐
Cu and W‐Ni‐Fe alloys. Due to their combinations of high density, strength, and ductility …

[图书][B] High-pressure shock compression of solids

JR Asay, M Shahinpoor - 2012 - books.google.com
This book presents a set of basic understandings of the behavior and response of solids to
propagating shock waves. The propagation of shock waves in a solid body is accompanied …

Processing strategy for consolidating tungsten heavy alloys for ordnance applications

A Upadhyaya - Materials Chemistry and Physics, 2001 - Elsevier
The environmental concern over the use of depleted uranium (DU) alloys as kinetic-energy
(KE) penetrator for high strain rate applications has focussed the interest in tungsten alloys …

Microstructure and mechanical properties of mechanically alloyed and solid-state sintered tungsten heavy alloys

HJ Ryu, SH Hong, WH Baek - Materials Science and Engineering: A, 2000 - Elsevier
The mechanical properties of solid-state sintered 93W–5.6 Ni–1.4 Fe tungsten heavy alloys
fabricated by mechanical alloying were investigated. Blended W, Ni and Fe powders were …

Combination of mechanical alloying and two-stage sintering of a 93W–5.6 Ni–1.4 Fe tungsten heavy alloy

SH Hong, HJ Ryu - Materials Science and Engineering: A, 2003 - Elsevier
The microstructural evolution and mechanical properties of a mechanically alloyed and two-
stage sintered tungsten heavy alloy were investigated. Elemental powders of tungsten …

Sintering time and atmosphere influences on the microstructure and mechanical properties of tungsten heavy alloys

RM German, A Bose, SS Mani - Metallurgical Transactions A, 1992 - Springer
The mechanical properties of tungsten heavy alloys are sensitive to the processing cycle
and are adversely affected by residual porosity. Sintering times greater than 2 hours usually …

Refractory metal alloying: A new method for improving mechanical properties of tungsten heavy alloys

UR Kiran, A Panchal, MP Kumar… - Journal of Alloys and …, 2017 - Elsevier
Influence of mechanically alloyed tungsten-rhenium powders on the microstructure and
mechanical properties of liquid phase sintered 89W-7Ni-3Fe-1Re heavy alloy was studied …

Fine-grained 93W–5.6 Ni–1.4 Fe heavy alloys with enhanced performance prepared by spark plasma sintering

Y Li, K Hu, X Li, X Ai, S Qu - Materials Science and Engineering: A, 2013 - Elsevier
Blended 93W–5.6 Ni–1.4 Fe powders were sintered via the spark plasma sintering (SPS)
technique. Fine-grained 93W–5.6 Ni–1.4 Fe heavy alloys (W grain size is about 6µm) with …

Tensile behavior change depending on the varying tungsten content of W–Ni–Fe alloys

IS Humail, F Akhtar, SJ Askari, M Tufail, X Qu - International Journal of …, 2007 - Elsevier
Tungsten heavy alloys (WHAs) are metal–metal composites consisting of nearly pure
spherical tungsten particles embedded in a Ni–Fe–W or Ni–Co–W or Ni–Cu–W ductile …