Z Kanwal, MN Usmani - Materials Research Express, 2018 - iopscience.iop.org
Current study is based on PBE-GGA and GGA+ U computational approach for calculating optical properties of Mn doped CdS. Cd atom in host CdS lattice (rocksalt structure) are …
SK Gaur, A Chaudhary, Q Murtaza… - Journal of Molecular …, 2025 - Elsevier
CdS nanoscale thin films were deposited on glass substrates at 1, 5 and 10 Å/s deposition rates by thermal evaporation process. The structural, morphological, compositional, optical …
A Kennedy, K Viswanathan - Physics Letters A, 2016 - Elsevier
Abstract The Zn-doped MnIn 2 S 4 thin films were deposited by chemical spray pyrolysis technique on a heated glass substrate using the aqueous solution of MnCl 2, InCl 3,(NH 2) 2 …
MJI Khan, Z Kanwal - Materials Research Express, 2018 - iopscience.iop.org
In current research, we perform a computational study to calculate optical properties of Al doped CdS system for 1× 1× 2, 2× 2× 1, 2× 2× 2 supercell configurations and for DFT+ U (1× …
The demands for energy are getting bigger with the increasing of the development of life's technology. The renewable sources of energy are connected to the main one which is solar …
A Kennedy, VS Kumar, KP Raj - Journal of Physics and Chemistry of Solids, 2017 - Elsevier
Bismuth (Bi)-doped manganese indium sulphide (MnInS 4) thin films were deposited on heated glass substrates using an aqueous solution of MnCl 2, InCl 3,(NH 2) 2 CS and BiCl 3 …
ARA Ridha, NA Al-Isawi - Journal of Physics: Conference Series, 2019 - iopscience.iop.org
In the present study, thermal evaporation technique in vacuum has been use to prepare CdS thin films doped with 1% Cu nanoparticles with average particles sizes 50 nm. The effect of …
Thermal evaporation technique is used to deposit CdS thin films on glass substrates using CdS powder. Various characterization techniques have been used to investigate the …
CdSe: 1% Ag thin films prepared by thermal evaporation method on glass substrates under vacuum technique with rate of deposition equal to 50 nm/min, the deposited films thickness …