Tensile strength of thermally modified laminated strand lumber and laminated veneer lumber

MD Aro, X Wang, DE McDonald… - Wood Material Science & …, 2017 - Taylor & Francis
Laminated strand lumber (LSL) and laminated veneer lumber (LVL) were thermally modified
as a post-treatment at 140° C, 150° C, 160° C, 170° C, and 180° C. The tension modulus of …