[HTML][HTML] Current status on lithium disilicate and zirconia: a narrative review

F Zarone, MI Di Mauro, P Ausiello, G Ruggiero… - BMC oral health, 2019 - Springer
Background The introduction of the new generation of particle-filled and high strength
ceramics, hybrid composites and technopolymers in the last decade has offered an …

A brief review on fatigue test of ceramic and some related matters in Dentistry

LF Valandro, AC Cadore-Rodrigues… - Journal of the …, 2023 - Elsevier
The characteristics of dental ceramics have been extensively studied over the years to
provide highly qualified materials for use in prosthetic restorations. The ability to adhere to …

CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: Fatigue performance and ceramic surface …

R Schestatsky, CP Zucuni, AB Venturini… - Journal of the …, 2019 - Elsevier
To evaluate the fatigue failure load (FFL), number of cycles for failure (CFF) and survival
probabilities of lithium-disilicate (LD) monolithic crowns manufactured by two processing …

Does Adhesive Luting Reinforce the Mechanical Properties of Dental Ceramics Used as Restorative Materials? A Systematic Review and Meta-Analysis.

LS da Rosa, KS Dapieve, F Dalla-Nora… - The Journal of …, 2022 - europepmc.org
Purpose This systematic review aims to explore and compile the effect of adhesive luting on
the mechanical properties of dental ceramics used as restorative materials. Materials and …

Do resin cement viscosity and ceramic surface etching influence the fatigue performance of bonded lithium disilicate glass-ceramic crowns?

KS Dapieve, GKR Pereira, AB Venturini, N Daudt… - Dental Materials, 2022 - Elsevier
Objective To assess the effects of a resin cement in high and low viscosity and distinct
conditioning of the intaglio surface of lithium disilicate glass-ceramic crowns on fatigue …

Influence of preparation designs on marginal adaptation and failure load of full‐coverage occlusal veneers after thermomechanical aging simulation

D Angerame, M De Biasi, M Agostinetto… - Journal of Esthetic …, 2019 - Wiley Online Library
Objectives To evaluate the fracture resistance and marginal quality of maxillary molars
restored using lithium disilicate glass‐ceramic (LDG) occlusal veneers with two preparation …

Cyclic fatigue tests on non-anatomic specimens of dental ceramic materials: a scoping review

HC Velho, KS Dapieve, LF Valandro… - Journal of the …, 2022 - Elsevier
The aim of the present scoping review was to identify and discuss the methods, testing
parameters, and characteristics used to induce cyclic fatigue on non-anatomic dental …

Effect of hydrofluoric acid concentration and etching time on the adhesive and mechanical behavior of glass-ceramics: A systematic review and meta-analysis

BVP Riesgo, C da Silva Rodrigues… - International Journal of …, 2023 - Elsevier
Statement of problem The process prior to cementing a glass ceramic requires that the
surface be etched with hydrofluoric acid in order to improve its adhesion. HF acid …

Metal center ion effects on photoinactivating rapidly growing mycobacteria using water-soluble tetra-cationic porphyrins

KB Guterres, GG Rossi, MMA de Campos, KS Moreira… - Biometals, 2020 - Springer
Rapidly growing mycobacteria (RGM) are pathogens that belong to the mycobacteriaceae
family and responsible for causing mycobacterioses, which are infections of opportunistic …

Adhesion to lithium disilicate glass-ceramics after aging: Resin viscosity and ceramic surface treatment effects

KS Dapieve, RO Pilecco, RW Temp, MA Villetti… - Journal of the …, 2023 - Elsevier
Objective To evaluate the influence of intaglio ceramic surface treatments, resin cement
viscosities, and storage regimens on the microshear bond strength of lithium disilicate …