B Sun, D Wang, X Lu, D Wan, D Ponge… - Acta Metallurgica Sinica …, 2021 - Springer
Hydrogen embrittlement (HE) is one of the most dangerous yet most elusive embrittlement problems in metallic materials. Advanced high-strength steels (AHSS) are particularly prone …
J Hu, XY Li, QW Meng, LY Wang, YZ Li, W Xu - Materials Science and …, 2022 - Elsevier
Medium Mn steels are promising candidates for the third-generation advanced high strength steels. However, it shows a distinct limit of mechanical property under conventional hot …
Medium Mn steels possess a composite like microstructure containing multiple phase constituents like metastable austenite, ferrite, δ-ferrite and α′-martensite with a wide range …
B Mishra, V Singh, R Sarkar, A Mukhopadhyay… - Materials Science and …, 2022 - Elsevier
In present study two different austenitic based low-density steel (LDS) grades with compositions of Fe–28Mn–9Al-0.9 C and Fe–15Mn–9Al-0.9 C–5Ni (in weight percent) were …
B Sun, F Fazeli, C Scott, N Brodusch, R Gauvin, S Yue - Acta Materialia, 2018 - Elsevier
The present study systematically investigated the effect of Si additions from 0 to 3 wt.% on the deformation mechanisms of a 0.2 C-10Mn-3Al medium Mn steel. Two austenite-ferrite …
B Sun, N Vanderesse, F Fazeli, C Scott, J Chen… - Scripta Materialia, 2017 - Elsevier
The correlation between the strain-induced martensite transformation (SIMT) and the Portevin-Le Chatelier (PLC) effect during tensile testing of a ferrite-austenite duplex medium …
Al x CoCrFeNi high entropy alloys (HEAs) with Al molar ratios of 0.3, 0.6 and 0.9 were subjected to hot plane strain compression testing at varying strain rates and strains in the …
Manganese is normally considered as the most important alloying element in medium Mn steels. However, the influence of Mn additions on the microstructural characteristics and the …
AK Da Silva, G Leyson, M Kuzmina, D Ponge, M Herbig… - Acta Materialia, 2017 - Elsevier
We investigated a high-purity cold-rolled martensitic Fe-9wt% Mn alloy. Tensile tests performed at room temperature after tempering for 6 h at 450° C showed discontinuous …