Wear and fatigue behaviour of deep cryogenically treated H21 tool steel

D Korade, KV Ramana, K Jagtap - Transactions of the Indian Institute of …, 2020 - Springer
The influence of deep cryotreatment before and after double tempering on hardness, wear
rate, surface finish and fatigue limit of AISI H21 tool steel has been examined. In the present …

[HTML][HTML] Influence of cryogenic treatment on the tribological behaviour of AISI H21 tool steel

D Korade, KV Ramana, K Jagtap - Materials Research, 2018 - SciELO Brasil
The aim of the present work was to find out the optimum cryosoaking duration of deep
cryogenic treatment to reduce the wear rate. The AISI H21 hot work tool steel specimens …

Effect of carbide density on fatigue limit of H21 die steel

DN Korade, KV Ramana, KR Jagtap - Journal of Materials Engineering …, 2020 - Springer
In the present work, the effect of carbide density on microstructure, hardness, wear rate, and
fatigue limit of AISI H21 die steel has been studied. The specimens of H21 die steel have …

Особенности формирования структуры, эксплуатационных свойств и качества поверхностного слоя штамповой оснастки из стали 3Х2В8Ф

НС Улаханов, УЛ Мишигдоржийн, АД Грешилов… - iPolytech …, 2019 - cyberleninka.ru
Целью статьи является исследование формирования эксплуатационных свойств и
параметров качества поверхностного слоя штамповой стали 3Х2В8Ф, используемой …

Modeling the Precipitation Kinetics of Cementite in Bainite in 0.17% Carbon Steel

Y Yang, B Wang, ZD Wang, YM Li, GD Wang… - Materials Science …, 2017 - Trans Tech Publ
Nanoscale cementite can be obtained in 0.17% carbon steel during isothermal treatment at
500oC after ultra fast cooling (UFC) and thermo-mechanical treatment. The precipitation …

[引用][C] Experimental investigation of deep cryogenic treatment of H21 tool steel

KD Nanasaheb - 2019 - Vaddeswaram