[HTML][HTML] Formation mechanism of MnS inclusion during heat treatments and its influence on the pitting behavior of 316L stainless steel fabricated by laser powder bed …

Z Duan, C Man, H Cui, Z Cui, X Wang - Corrosion Communications, 2022 - Elsevier
The formation mechanism of MnS inclusions during heat treatment and its effect on the
pitting behavior of laser powder bed fusion (L-PBF)-fabricated 316L stainless steel (SS) …

Analysis of MnS inclusions formation in resulphurised steel via modeling and experiments

H Liu, D Hu, J Fu - Materials, 2019 - mdpi.com
Controlling the formation of MnS inclusions during solidification influences the mechanical
properties and machinability of the resulfurized steel. A coupled segregation–nucleation …

[HTML][HTML] On the mechanical properties and deformation mechanisms of manganese sulphide inclusions

CF Kusche, JSKL Gibson, MA Wollenweber… - Materials & Design, 2020 - Elsevier
Manganese sulphide (MnS) inclusions are present in many steels. Some are deliberately
introduced to increase machinability (Ånmark et al., 2015 [1]), for example in case-hardened …

[HTML][HTML] Examining the Effect of MnS Particles on the Local Deformation Behavior of 8MnCrS4-4-13 Steel by In Situ Tensile Testing and Digital Image Correlation

F Qayyum, SC Tseng, S Guk, F Hoffmann… - Journal of Composites …, 2023 - mdpi.com
In this study, the behavior of MnS particles in a steel matrix is investigated through in situ
tensile testing and digital image correlation (DIC) analysis. The goal of this research is to …

[HTML][HTML] Effect of Ti and S Content on the Properties and Machinability of Low-Carbon Ferritic–Pearlitic Steel

B Arh, F Tehovnik, F Vode, B Podgornik - Metals, 2024 - mdpi.com
This research was focused on the effect of Ti and S content on the formation of non-metallic
inclusions and their influence on the mechanical properties and machinability of low-carbon …

Role of non-metallic inclusions in the fracture behavior of cold drawn pearlitic steel

J Toribio, FJ Ayaso, B González - Metals, 2021 - mdpi.com
In this paper an exhaustive scientific work is performed, by means of metallographic and
scanning electron microscope (SEM) techniques, of the microstructural defects exhibited by …

Evolution of non-metallic inclusions with cold drawing in progressively cold drawn eutectoid pearlitic steel wires

J Toribio, FJ Ayaso, R Rodríguez - Procedia Structural Integrity, 2021 - Elsevier
This article focuses on the analysis of the evolution of inclusions present in eutectoid
pearlitic steel subjected to a real cold drawing process. To this end, wires belonging to …

Study on defect reduction in casting of Ni-Cr alloy (UNS N06003)

K Samvatsar, H Dave - IOP Conference Series: Materials Science …, 2022 - iopscience.iop.org
In modern times, selection criteria of materials are solely based on its utilization. The
characteristics of materials like high temperature sustainability with regard to its strength and …

Drawing-Induced Evolution of Inclusions in Cold-Drawn Pearlitic Steel

J Toribio, FJ Ayaso, R Rodriguez - Metals, 2021 - mdpi.com
This article focuses on the analysis of the evolution of inclusions present in eutectoid
pearlitic steel subjected to a real cold drawing process. To this end, wires belonging to …

Effect of addition of calcium-based reagents on defect reduction of cast Fe-Ni-Cr alloy

H Dave, K Samvatsar - Advances in Materials and Processing …, 2023 - Taylor & Francis
ABSTRACT UNS N08120, a member of Fe-Ni-Cr alloy family, is capable to withstand severe
high temperature and corrosive environments for applications in chemical, power, waste …