Hot workability investigation of an Fe-Al-Ta alloy using deformation processing maps

A Emdadi, H Michels, M Tovar - Metals, 2023 - mdpi.com
Fe-Al-Ta alloys are expected to replace high-alloyed steels in steam turbine blades.
However, the mechanical properties of the forged blades are still not optimal due to limited …

On the hot deformation of a Fe-Al-Ta iron aluminide prepared via laser powder bed fusion

A Emdadi, S Bolz, F Jensch, M Tovar, S Weiß - Crystals, 2023 - mdpi.com
In the present work, a combined process of laser powder bed fusion (LPBF) and hot working
in terms of microstructure refinement was investigated for Fe-25Al-1.5 Ta alloy samples …

The role of (Fe, Al) 2Nb Laves phase on the high temperature oxidation behaviour of intermetallic Fe–26Al–4Nb iron aluminide

RD Pütz, D Zander - Intermetallics, 2023 - Elsevier
The role of the (Fe, Al) 2 Nb Laves phase on the high temperature oxidation mechanisms of
Fe–26Al–4Nb (at%) was investigated between 700° C and 1000° C in air for 500 h. The (Fe …

A comparative study of microstructure and hot deformability of a Fe–Al–Ta iron aluminide prepared via additive manufacturing and conventional casting

A Emdadi, S Weiß - Crystals, 2022 - mdpi.com
In this work, the microstructure and hot deformation behavior of laser powder bed fusion (L-
PBF) and conventionally cast Fe-25Al-1.5 Ta (at.%) alloys were compared. The L-PBF builds …

Ti6Al4V alloy remelting by modulation laser: Deep penetration, high compactness and metallurgical bonding with matrix

L Shen, Y Chen, H Zhu, Y Lei, C Qiu - Micromachines, 2022 - mdpi.com
Titanium alloys are famous for their light weight, high strength, and heat-and corrosion-
resistant properties. However, the excellent mechanical properties are closely related to its …

[HTML][HTML] Stress relief heat treatment and mechanical properties of laser powder bed fusion built 21-6-9 stainless steel

E Edin, F Svahn, M Neikter, P Åkerfeldt - Materials Science and …, 2023 - Elsevier
In this work, the effectiveness of residual stress relief annealing on a laser powder bed
fusion (L-PBF) manufactured austenitic stainless steel, alloy 21-6-9 was investigated …

Effects of boriding and aluminizing on the electrochemical and wear behavior of IN-718 nickel-based alloy

Z Tang, C Yang, Y Duan, L Ma, S Zheng… - Surface and Coatings …, 2024 - Elsevier
Due to the distinct surface coating properties of IN-718 nickel-based alloy after boriding and
aluminizing treatments, a comparative study was conducted. Optimal process parameters for …

High-temperature hardness and scratch behaviour of differently strengthened iron aluminide laser claddings

H Rojacz, K Pichelbauer, M Varga… - Surface and Coatings …, 2024 - Elsevier
Fe 3 Al-based iron aluminides provide notable high-temperature properties at a
comparatively low overall ecological impact. To improve their wear resistance, different …

[HTML][HTML] Hot Working of an Fe-25Al-1.5 Ta Alloy Produced by Laser Powder Bed Fusion

A Emdadi, S Bolz, S Weiß - Crystals, 2023 - mdpi.com
In the present work, hot working was used as a post-processing method for Fe-25Al-1.5 Ta
(at.%) alloy built using laser powder bed fusion (LPBF) to refine the undesirable columnar …

[HTML][HTML] Hot deformation behavior of a Fe3Al–Ta alloy in the B2-order regime

A Emdadi, M Tovar, A Jedynak, S Weiß - Intermetallics, 2024 - Elsevier
Highlights•Hot deformation behavior of Fe–25Al-1.5 Ta alloy in the ordered B2-phase