Effect of boron-based glass additives on the ionic conductivity of Li1. 3Al0. 3Ti1. 7 (PO4) 3 solid electrolyte

J Kang, X Guo, R Gu, Y Tang, H Hao, Y Lan… - Journal of Alloys and …, 2023 - Elsevier
Abstract Li 1.3 Al 0.3 Ti 1.7 (PO 4) 3 (LATP) is a promising candidate as the solid electrolyte
in energy storage devices. For practical considerations, the most common ways to …

Al/Al2O3 Composite Coating Deposited by Flame Spraying for Marine Applications: Alumina Skeleton Enhances Anti-Corrosion and Wear Performances

J Huang, Y Liu, J Yuan, H Li - Journal of thermal spray technology, 2014 - Springer
Here we report aluminum-alumina composite coatings fabricated by flame spraying for
potential marine applications against both corrosion and wear. Microstructure examination …

Microstructural features, physicο‐mechanical properties, and wear behavior of dental translucent polychromic multilayer zirconia of hybrid composition prepared by …

K Dimitriadis, M Constantinou… - Journal of Esthetic …, 2023 - Wiley Online Library
Objective The present study determined the mechanical properties and the wear behavior,
as results of the micro (nano) structure, of the enamel, transition, and dentine layers, which …

Fabrication of nanodiamond reinforced aluminum composite coatings by flame spraying for marine applications

Y Fu, X Chen, B Zhang, Y Gong, H Zhang… - Materials Today …, 2018 - Elsevier
Thermal sprayed aluminum (Al) coatings have been extensively utilized for marine
anticorrosion applications. However, lack in mechanical strength of the coatings persists as …

Effects of processing parameters on microstructure and mechanical behavior of SiO2/Ti–6Al–4V joint brazed with AgCu/Ni interlayer

JC Feng, D Liu, LX Zhang, XC Lin, P He - Materials Science and …, 2010 - Elsevier
SiO2 glass ceramic has been successfully joined to Ti–6Al–4V alloy with AgCu/Ni composite
interlayer. The brazing temperature varies from 950° C to 980° C, with the holding time …

Development of high-performance enamel coating on grey iron by low-temperature sintering

D Song, R Tang, F Yang, Y Qiao, J Sun, J Jiang, A Ma - Materials, 2018 - mdpi.com
In this study, we report on a low-temperature sintered enamel coating with a high-strength
bonding and wear-resistance that protected a grey cast iron substrate. The SiO2–Al2O3 …

Wear resistance glass-ceramics with a gahnite phase obtained in CaO-MgO-ZnO-Al2O3-B2O3-SiO2 system

D Herman, T Okupski, W Walkowiak - Journal of the European Ceramic …, 2011 - Elsevier
The thermal conditions for obtaining the glass-ceramic material of Al0. 107B0. 374Mg0.
043Zn0. 282Ca0. 100Si0. 927O3 with a crystalline phase in the form of gahnite (ZnAl2O4) …

Crystallization and microstructure in K2O substituted SiO2–MgO–Al2O3–Li2O–AlPO4 glass-ceramics

M Garai, CK Singh, SK Rout - Solid State Communications, 2022 - Elsevier
The substitution of K+ ion by Ca 2+ or Sr 2+ in K2O–SiO2–MgO–Al2O3–B2O3–MgF2–Li2O–
AlPO4 glass is executed and the relevant effects on crystallization and microstructure are …

Tribological behavior of alumina-added apatite–wollastonite glass–ceramics in simulated body fluid

J Park, SH You, DW Shin, A Ozturk - Materials Chemistry and Physics, 2010 - Elsevier
Tribological properties of an alumina-added apatite–wollastonite glass–ceramic produced
by controlled heat treatment of a glass in the system MgO–CaO–SiO2–P2O5–Al2O3 have …

Microstructural and wear behavior characterization of porous layers produced by pulsed laser irradiation in glass-ceramics substrates

D Sola, A Conde, I García, E Gracia-Escosa… - Materials, 2013 - mdpi.com
In this work, wear behavior and microstructural characterization of porous layers produced in
glass-ceramic substrates by pulsed laser irradiation in the nanosecond range are studied …