[HTML][HTML] Review of laser powder bed fusion (LPBF) fabricated Ti-6Al-4V: process, post-process treatment, microstructure, and property

S Cao, Y Zou, CVS Lim, X Wu - Light: Advanced Manufacturing, 2021 - light-am.com
Laser powder bed fusion (LPBF) is a timely important additive manufacturing technique that
offers many opportunities for fabricating three-dimensional complex shaped components at …

ASB induced phase transformation in high oxygen doped commercial purity Ti

W Shi, S Lu, J Shen, B Chen, J Umeda, Q Wei… - Materials Science and …, 2022 - Elsevier
Given that commercial purity titanium (CP-Ti) doped with a high oxygen concentration has
recently been reported with high mechanical performance, the present work investigated the …

Different effects of multiscale microstructure on fatigue crack growth path and rate in selective laser melted Ti6Al4V

Z Qi, B Wang, P Zhang, R Liu, Z Zhang… - Fatigue & Fracture of …, 2022 - Wiley Online Library
During the selective laser melting (SLM) process of Ti6Al4V, a special structure can be
formed with columnar prior β grains along the building direction and fully martensitic α …

Laser powder bed fusion produced Ti-6Al-4V: Influence of high-energy process parameters on in-situ martensite decomposition and prior beta grain texture

GM Ter Haar, TH Becker - Journal of Alloys and Compounds, 2022 - Elsevier
Abstract Since Ti-6Al-4V components fabricated by laser powder bed fusion achieve an
undesired martensitic microstructure (α'), high residual stresses and columnar prior-β grains …

The influence of microstructural texture and prior beta grain recrystallisation on the deformation behaviour of laser powder bed fusion produced Ti-6Al-4V

GMT Haar, TH Becker - Available at SSRN 3694108, 2020 - papers.ssrn.com
The control and predictability of mechanical properties during manufacturing is essential in
achieving parts that consistently deliver adequate mechanical properties. In laser powder …

Laser powder bed fusion produced Ti-6AI-4V: microstructural transformations and changes in deformation behaviour through thermal treatments.

G Ter Haar - 2021 - scholar.sun.ac.za
The current 4th Industrial Revolution has brought about enormous potential for social-
economic development in South Africa. Additive manufacturing, a key technology of the 4th …

Tailoring Heat Treatments for Metals Processed by Laser Powder Bed Fusion

P Van Cauwenbergh - 2022 - lirias.kuleuven.be
The project's main goal is to design tailored post-process heat treatments for four LPBF high-
end alloys (AlSi10Mg, AlSi7Mg, Ti6Al4V ELI, Inconel 718) that are widely used in the …

Choosing a suitable heat treatment regime for stress-relief and microstructure stabilization of ti6al4v alloy 3d-printed by slm method

M Roudnická, EA Tarquino… - Defect and Diffusion Forum, 2020 - Trans Tech Publ
During the processing of Ti6Al4V alloy by a 3D printing method SLM (selective laser
melting), high internal stresses are developed in the material as a result of high temperature …

Performance assessment of a ti6al4v (eli) light aircraft nose wheel fork produced through laser powder bed fusion

HP Miya - 2023 - ir.cut.ac.za
A scaled-down nose wheel fork for a light aircraft was redesigned by applying topology
optimization for manufacturing in Ti6Al4V (ELI) through laser powder bed fusion (LPBF) …

Microstructural and Mechanical Analysis of High-Performance Parts Produced by Hybrid Additive Manufacturing of Powder LMD on Forged Base Components

S Hemes, W Koch, R Hama-Saleh, I Sizova… - Advanced Materials …, 2021 - Trans Tech Publ
Ti-6Al-4V is used as a high-performance material in many industries (mainly automotive and
aerospace, but also the medical industry) and traditionally produced by hot forging, with …