MC García-Alonso, B Chico, RM Lozano… - Tribology …, 2023 - Elsevier
In this work graphene-based solid lubricants biofunctionalized with hyaluronic acid were deposited on CoCr surfaces to decrease wear-corrosion phenomena. Graphene oxide was …
S Montalvo, S Fouvry, M Martinez - Wear, 2024 - Elsevier
Fretting fatigue causes failures in steel wire ropes. These steel wires are usually galvanised. This zinc coating could change the crack initiation process, as it modifies the contact …
This paper reports an investigation into the deployment of a thin layer of tin as a lubricant on low carbon steel tube for tube drawing process. The layer was deposited using electro …
In this work, a superhydrophobic top coating was applied to an A653 hot-dipped galvanized steel. Nanoindentation tests were performed to measure hardness and the ratio of hardness …
In this paper, the tin coating layer is utilized as a solid lubricant for the cold steel tube drawing process. The effect of different thicknesses of tin coatings as a tribo-layer has been …
For severe metal deformation processes such as metal drawing operations, the use of porous lubricant carrier layer on metal surfaces has been proposed in recent literature for …