Polished specimens of AA2024-T3 alloy were immersed for up to 120min in 0.1 M NaCl. The development of corrosion was monitored using scanning electron microscopy with energy …
Optical and electron microscopies and EBSD were used to study the early stages of corrosion propagation during stable pit formation on AA2024-T3. Polished AA2024-T3 …
DR Gunasegaram… - International materials …, 2014 - journals.sagepub.com
Localised corrosion is a cause of unanticipated and sometimes catastrophic failures of equipment, transport vessels and infrastructures. Therefore, the development of modern …
H Kakinuma, I Muto, Y Oya, T Momii… - Journal of The …, 2021 - iopscience.iop.org
The relationship between the change in the open-circuit potential (OCP) and the morphology of metastable pitting at Al–Fe–Si particles of AA1050 aluminum in 0.1 M NaCl …
B Malki, G Berthomé, T Souier, C Boissy… - Journal of the …, 2021 - iopscience.iop.org
In the present work, a dual experimental and computational technique is used to study crevice corrosion of ferritic stainless steels in chloride-containing media. A specifically …
High strength aluminium alloy AA2024 is susceptible to localized corrosion in the form of pitting and intergranular corrosion (IGC). The corrosion behaviour of this alloy is strongly …
PJ Skrdla - Physical Chemistry Chemical Physics, 2010 - pubs.rsc.org
Oscillatory kinetic behavior is reported for the first time in a solid-state phase transformation of an organic compound, specifically, in the dissolution of Form V crystals of etoricoxib in …
Aluminium and its alloys are considered to be the most versatile engineering materials across a broad range of applications [1-15]. Aluminium is a key component in so many …