The lithium-ion battery (LIB) has been the dominant technology in the rechargeable energy storage market for more than twenty years. However, to meet the increasing need for electric …
L Hallmann, P Ulmer, M Kern - Journal of the mechanical behavior of …, 2018 - Elsevier
The mechanical properties of lithium disilicate glass-ceramics depend on various factors, a prominent one being their microstructure. The aim of this review article is to elucidate the …
Nucleation is one of the primary contributions to the microstructure of glass-ceramics. However, the nucleation process within glass-ceramics is not understood across all glass …
A Vichi, RF Fonzar, C Goracci… - Operative …, 2018 - meridian.allenpress.com
Objective: To assess the efficacy of dedicated finishing/polishing systems on roughness and gloss of VITA Suprinity and IPS e. max CAD. Method: A total of 24 blocks of Suprinity and 24 …
Along with the rapid and extensive advancements in the 3D printing field, a diverse range of uses for 3D printing have appeared in the spectrum of medical applications. Vat …
N Monmaturapoj, P Lawita… - Advances in Materials …, 2013 - Wiley Online Library
This work proposes four different glass formulas derived from the SiO2‐Li2O‐K2O‐Al2O3 system to investigate the effect of glass composition on their crystal formations and …
HR Fernandes, DU Tulyaganov… - Journal of materials …, 2013 - Springer
The aim of this study was to investigate the effects of different nucleating agents (P 2 O 5, TiO 2 and ZrO 2) on the crystallization behaviour and the properties of a parent glass with …
K Chen, Y Li, X Meng, L Meng, Z Guo - Ceramics International, 2019 - Elsevier
Titanium-bearing blast furnace slag (TBBFS), which contains 15–30 wt% TiO 2, is a by- product of the iron-making process and is discharged at approximately 1500° C. To …
K Yuan, F Wang, J Gao, X Sun, Z Deng, H Wang… - Journal of non …, 2013 - Elsevier
Glass-ceramics derived from the SiO2–Li2O–K2O–Al2O3–ZrO2–P2O5 system were produced by a two-stage sintering cycle with a primary thermal treatment at 700° C followed …