Over the past years, the interest in doped phosphor materials has been extensively studied, due to their potential in applications such as light emitting diodes (LEDs), photonic circuits …
Undoped and europium ion (Eu 3+) doped ZnO nanostructures were synthesized via the chemical bath deposition method and annealed afterwards in air at 700° C. The X-ray …
Abstract Ce 3+, Eu 3+ and Tb 3+ singly and triply doped ZnAl 2 O 4 nano-powders were successfully synthesized via the citrate sol-gel method. X-ray diffraction (XRD) analysis …
Applying scanning electron microscopy in transmission mode and grazing incidence X-ray diffraction, we investigated the spinel-forming solid-state reaction between crystalline ZnO …
A series of the undoped, 0.1% Ce 3+, 0.1% Eu 2+, 0.1% Tb 3+ singly doped and 0.1% Ce 3+, 0.1% Eu 2+, x% Tb 3+(0⩽ x⩽ 2%) triply doped MgAl 2 O 4 nanophosphors were …
MA Malimabe, BF Dejene, HC Swart… - Journal of Molecular …, 2020 - Elsevier
Zinc oxide (ZnO) undoped, doped and co-doped with Ce 3+ and Eu 3+ were synthesized by the chemical bath deposition method. The nanopowders were spread through a polyvinyl …
MA Malimabe, SV Motloung, TE Motaung… - Physica B: Condensed …, 2020 - Elsevier
In this study undoped, Ce 3+-, Eu 3+-doped and Ce 3+: Eu 3+ and co-doped ZnO nanopowders were synthesized by the chemical bath deposition (CBD) method. The …
We have successfully synthesized ZnO: xmol% Ce 3+(0≤ x≤ 10 mol%) doped nanopowders via the chemical bath deposition method (CBD) technique at low temperature …
SP Khambule, SV Motloung, TE Motaung, LF Koao… - Results in Optics, 2022 - Elsevier
Abstract Undoped and Sm 3+ doped ZnAl 2 O 4 nanopowders were synthesized using the co-precipitation method and annealed at 750℃ for 3.5 h. The aim of this study was to …