Tribology of polymeric solids and their composites

BJ Briscoe, SK Sinha - Wear–Materials, Mechanisms and …, 2005 - Wiley Online Library
The purpose of this chapter is to rationalize and highlight some important established
phenomena in polymer tribology. Explanations are presented, where appropriate, on the …

Contact size, frequency and cyclic normal force effects on Ti–6Al–4V fretting wear processes: An approach combining friction power and contact oxygenation

S Fouvry, P Arnaud, A Mignot, P Neubauer - Tribology International, 2017 - Elsevier
We present fretting wear analysis of a dry Ti-6Al-4V cylinder/plane contact, investigating
sliding frequency, contact size, and cyclic normal force effects. The investigation showed that …

Some considerations on the mitigation of fretting damage by the application of surface-modification technologies

Y Fu, J Wei, AW Batchelor - Journal of Materials Processing Technology, 2000 - Elsevier
Fretting is a surface-degradation process due to mechanical and chemical attack by small-
amplitude oscillatory movement between two contacting surfaces and it is intimately related …

Effect of groove surface texture on the fretting wear of Ti–6Al–4V alloy

J Wang, W Xue, S Gao, S Li, D Duan - Wear, 2021 - Elsevier
Groove surface textures with different orientations and spacings were prepared on the Ti–
6Al–4V alloy by using a laser. Fretting tests (rubbed with a Ti–6Al–4V ball) were conducted …

Rheology and flows of solid third bodies: background and application to an MoS1. 6 coating

S Descartes, Y Berthier - Wear, 2002 - Elsevier
After a short background history on solid third bodies, this paper proposes a tribological
approach for understanding how a contact takes place when first bodies are in relative …

Microhardness and wear resistance of Al2O3-TiB2-TiC ceramic coatings on carbon steel fabricated by laser cladding

Z Li, M Wei, K Xiao, Z Bai, W Xue, C Dong, D Wei… - Ceramics …, 2019 - Elsevier
Abstract Al 2 O 3-TiB 2-TiC ceramic coatings with high microhardness and wear resistance
were fabricated on the surfaces of carbon steel substrates by laser cladding using different …

Laboratory testing of displacement and load induced fretting

H Mohrbacher, JP Celis, JR Roos - Tribology international, 1995 - Elsevier
A conceptually new simulation system for the laboratory investigation of fretting wear is
described. Fretting vibrations are generated either directly by oscillating a linear relative …

Finite element, critical-plane, fatigue life prediction of simple and complex contact configurations

WS Sum, EJ Williams, SB Leen - International Journal of Fatigue, 2005 - Elsevier
A finite element based critical plane approach is developed incorporating the Smith–Watson–
Topper (SWT) multiaxial fatigue criterion. The approach is applied to a cylinder-on-flat …

The effect of surface regular microtopography on fretting fatigue life

A Volchok, G Halperin, I Etsion - Wear, 2002 - Elsevier
The possibility of increasing fretting fatigue life of a tribo-pair by laser surface texturing
technology is studied. An appropriate experimental fretting fatigue device is used to conduct …

Fretting corrosion running regime and damage mechanism evolution of zirconium alloy mated with Inconel 718 alloy in high temperature high pressure water …

LZ Kang, YH Lu, WW Bian, L Xin, YM Han - Tribology International, 2024 - Elsevier
Fretting corrosion behavior and damage mechanism of Zr-4 alloy mated with Inconel 718