Microstructure, fractography, and mechanical properties of Hardox 500 steel TIG-welded joints by using different filler weld wires

Z Zuo, M Haowei, M Yarigarravesh, AH Assari… - Materials, 2022 - mdpi.com
This paper deals with the effects of three low-carbon steel filler metals consisting of ferritic
and austenitic phases on the weld joints of the tungsten inert gas (TIG) welding of Hardox …

Improving the mechanical strength of ductile cast iron welded joints using different heat treatments

ESV Marques, FJG Silva, OC Paiva, AB Pereira - Materials, 2019 - mdpi.com
The main advantage of welding cast iron is to recover parts by repairing defects induced by
casting processes (porosities, etc.), before they enter their working cycle, as well as repair …

The effect of current strength on tensile strength and impact toughness of cast iron welded joints

W Wijoyo, M Mujahid, A Nurhidayat… - … : Jurnal Sains dan …, 2021 - jurnal.untirta.ac.id
Cast iron is a high-carbon iron-carbon alloy. Cast iron is difficult to weld because of the high
carbon concentration. A good connection necessitates the application of specific strategies …

Mechanical and microstructural analysis in the welding of ductile cast iron by TIG procedure, with different filler materials and air cooling

J Martínez Alcón, M Pascual Guillamón… - Revista de …, 2021 - riunet.upv.es
[EN] The present work analyses the strength and microstuctural variations of ductile cast iron
welded by means of the TIG technique, without heat treatment and using different filler …

Optimization on the electrical discharge machining (EDM) process parameters of aged AA7075/TiC metal matrix composites

P Rajendran, V Duraisamy… - Revista de …, 2023 - revistademetalurgia.revistas.csic.es
The need to optimize the process parameters in Electrical Discharge Machining (EDM) for
aged AA7075 Metal Matrix Composites (AAMMCs) is evident as it impacts various aspects …

Pengaruh Variasi Suhu PWHT Normalizing Pada Instalasi I Bracket Pasca Pengelasan FCAW

U Budiarto, AWB Santosa - Jurnal Teknik Perkapalan, 2024 - ejournal3.undip.ac.id
Dalam pengelasan konstruksi kapal material tidak hanya satu jenis saja bahkan ada dua
material yang berbeda di sambungkan. Baja grade A termasuk golongan baja low carbon …

[PDF][PDF] Mechanical and microstructural analysis in GJS 400-15 ductile iron welding with Fe-Ni as filler metal, carried out by smaw and TIG welding with different heat …

J Martínez-Alcón, MP Guillamón… - Dyna: Ingeniería e …, 2022 - revista-dyna.com
GJS 400-15 ductile cast iron has excellent physical-chemical, mechanical-structural and
manufacturability properties. However, it has notable limitations when it is subjected to …

Análisis mecánico y microestructural en soldaduras de fundición dúctil GJS 400-15 con Fe-Ni como metal de aporte realizadas mediante soldeo SMAW y TIG con …

J Martínez-Alcón, MP Guillamón… - DYNA-Ingeniería e …, 2022 - search.ebscohost.com
GJS 400-15 ductile cast iron has excellent physical-chemical, mechanical-structural and
manufacturability properties. However, it has notable limitations when it is subjected to …

Análisis mecánico y microestructural en soldadura de fundición dúctil, mediante procedimiento TIG, con diferentes materiales de aporte y enfriamiento al aire

JM Alcón, MP Guillamón… - Revista de …, 2021 - revistademetalurgia.revistas.csic.es
The present work analyses the strength and microstuctural variations of ductile cast iron
welded by means of the TIG technique, without heat treatment and using different filler …

A Study on the Repair of Fatigue Damage at Large Cast Iron structure using Cold Joint Method

SR Lee, DJ Lee, SS Cho - Journal of the Korea Academia …, 2019 - koreascience.kr
Large cast iron structures are used in casings and pipes in shipsand chemical plants.
Broken parts in the casings and pipescan result in failures even when stresses are below …