Joining of dissimilar materials

K Martinsen, SJ Hu, BE Carlson - Cirp Annals, 2015 - Elsevier
Emerging trends in manufacturing such as light weighting, increased performance and
functionality increases the use of multi-material, hybrid structures and thus the need for …

Review of aluminum-to-steel welding technologies for car-body applications

A Gullino, P Matteis, F D'Aiuto - Metals, 2019 - mdpi.com
Hybrid car bodies fabricated by joining parts made with steel and aluminum alloys are
becoming increasingly common. This provides an affordable mean to decrease the car …

Dissimilar friction welding of 6061-T6 aluminum and AISI 1018 steel: Properties and microstructural characterization

E Taban, JE Gould, JC Lippold - Materials & Design (1980-2015), 2010 - Elsevier
Joining of dissimilar materials is of increasing interest for a wide range of industrial
applications. The automotive industry, in particular, views dissimilar materials joining as a …

A review on resistance spot welding of aluminum alloys

SM Manladan, F Yusof, S Ramesh, M Fadzil… - … International Journal of …, 2017 - Springer
This paper presents a review on the resistance spot welding (RSW) of Al/Al alloys, Al
alloys/steel, Al/Mg alloys, and Al/Ti alloys, with focus on structure, properties, and …

Dissimilar welding of carbon steel to 5754 aluminum alloy by Nd: YAG pulsed laser

MJ Torkamany, S Tahamtan, J Sabbaghzadeh - Materials & Design, 2010 - Elsevier
Laser welding of low carbon steel to 5754 aluminum alloy was studied in keyhole welding
mode in steel-on-aluminum overlap configuration. In order to decrease formation of …

Self-pierce riveting for sheet materials: state of the art

X He, I Pearson, K Young - Journal of materials processing technology, 2008 - Elsevier
Self-pierce riveting (SPR) is a high-speed mechanical fastening technique for point joining
of sheet materials. It is used heavily in the automotive sector due to the growing use of …

Effect of weld nugget size on overload failure mode of resistance spot welds

M Pouranvari, HR Asgari, SM Mosavizadch… - … and Technology of …, 2007 - Taylor & Francis
In the present paper, effects of welding current, welding time, electrode pressure and
holding time on the weld nugget size were studied. A failure mechanism was proposed to …

Failure mode transition in AHSS resistance spot welds. Part I. Controlling factors

M Pouranvari, SPH Marashi - Materials Science and Engineering: A, 2011 - Elsevier
Failure mode of resistance spot welds is a qualitative indicator of weld performance. Two
major types of spot weld failure are pull-out and interfacial fracture. Interfacial failure, which …

Dissimilar metal joining of aluminum alloy to galvanized steel with Al–Si, Al–Cu, Al–Si–Cu and Zn–Al filler wires

H Dong, W Hu, Y Duan, X Wang, C Dong - Journal of Materials Processing …, 2012 - Elsevier
Aluminum alloy sheets were lap joined to galvanized steel sheets by gas tungsten arc
welding (GTAW) with Al–5% Si, Al–12% Si, Al–6% Cu, Al–10% Si–4% Cu and Zn–15% Al …

An overview of self-piercing riveting process with focus on joint failures, corrosion issues and optimisation techniques

HQ Ang - Chinese Journal of Mechanical Engineering, 2021 - Springer
Self-piercing riveting (SPR) is a cold forming technique used to fasten together two or more
sheets of materials with a rivet without the need to predrill a hole. The application of SPR in …